Minghsin University Institutional Repository:Item 987654321/142
English  |  正體中文  |  简体中文  |  Items with full text/Total items : 1365/1366 (100%)
Visitors : 1334524      Online Users : 805
RC Version 7.0 © Powered By DSPACE, MIT. Enhanced by NTU Library IR team.
Scope Tips:
  • please add "double quotation mark" for query phrases to get precise results
  • please goto advance search for comprehansive author search
  • Adv. Search
    HomeLoginUploadHelpAboutAdminister Goto mobile version


    Please use this identifier to cite or link to this item: http://120.105.36.38/ir/handle/987654321/142


    Title: 銀銅雙金屬活性碳粉體觸媒之製備及應用於一氧化氮空氣污染物還原
    Authors: 陳利強
    Contributors: 化學工程與材料科技系
    Keywords: 活性碳,銀銅雙金屬,一氧化氮,還原反應
    Date: 2008-12
    Issue Date: 2010-03-23 16:35:27 (UTC+8)
    Abstract: 本研究以化學含浸法,利用硝酸銀及硝酸銅將銀及銅活性相,依一定比例(銀:銅=100:0, 80:20, 60:40, 40:60, 20:80, 0:100)置入活性碳擔體中,製成銅銀雙金屬活性碳粉体觸媒,再測試該系列觸媒應用於一氧化氮(NO)空氣污染物的還原特性,其NO還原性能係在無氨環境下以一固定床式反應器進行測試。測試條件的改變範圍包含:改變銀添加量、改變銀與銅的添加比例、有或無預氧化、改變反應溫度(180~450℃)等因子,研究之目的為改良活性碳/NO還原反應,作為發展以活性碳觸媒法還原一氧化氮空氣污染物技術之參考。
    實驗結果發現預氧化對觸媒NO轉化率有明顯影響,對未添加銀之添加100%銅的活性碳觸媒而言,有預氧化的觸媒其NO轉化率明顯高於無預氧化者;但是對含有銀成份的活性碳觸媒而言,無預氧化的觸媒其NO轉化率反而高於有預氧化者;因此可建議凡添加銀的活性碳觸媒,可省去預氧化的製作步驟。由實驗比較各式銀銅雙金屬活性碳觸媒的一氧化氮還原性能可知,在有預氧化的條件下添加100%銅的活性碳觸媒具有最佳的NO轉化率;而在無預氧化條件下銅銀添加比例為Cu:Ag=75:25的觸媒具有最佳的NO還原性能。
    Appears in Collections:[Department of Chemical and Materials Engineering] Research Projects in School

    Files in This Item:

    File Description SizeFormat
    陳利強.pdf755KbAdobe PDF2768View/Open


    All items in MUSTIR are protected by copyright, with all rights reserved.


    DSpace Software Copyright © 2002-2004  MIT &  Hewlett-Packard  /   Enhanced by   NTU Library IR team Copyright ©   - Feedback